ASTM 321 Cold Rolled Stainless Steel Sheet SS Plate 14 Gauge 2B Finish
Product Details:
Place of Origin: | China |
Brand Name: | TISCO,BAOSTEEL,POSCO,JISCO,LISCO |
Certification: | MTC; SGS |
Model Number: | 321 |
Payment & Shipping Terms:
Minimum Order Quantity: | 1 Ton |
---|---|
Price: | Negotiable |
Packaging Details: | waterproof paper and steel strip reinforcement,one package about 2 tons,Load in 20' or 40' GP |
Delivery Time: | 10-15 working days |
Payment Terms: | L/C, T/T, Western Union, D/A |
Supply Ability: | 200 tons per month |
Detail Information |
|||
Name: | Austenite 12 Gauge 304L 321 Plate | Surface: | 2B |
---|---|---|---|
Technique: | Cold Rolled | Price Term: | FOB, CFR, CIF |
Packing: | Standard Sea-worthy Packing | Application: | Decoration, Construction |
Thickness: | 2.78 Mm | Grade: | BS EN 1.4306, 1.4541 |
Width: | 1000,1219, 1250 | Length: | 2000,2438,3000,6000 |
High Light: | ASTM 321 Stainless plate Sheet,14 Gauge 2B Stainless plate Sheet,Austenite Stainless plate Sheet |
Product Description
Cold Rolled Stainless Steel Sheet ASTM 321 SS Plate 14 Gauge 2B finish
Model 321 -- SIMILAR TO 304 EXCEPT THAT THE RISK OF MATERIAL WELD CORROSION IS REDUCED DUE TO THE ADDITION OF TITANIUM.
Product introduction:
Commodity | Cold Rolled Stainless Steel Sheet ASTM 321 SS Plate 14 Gauge 2B finish |
Grade | 321 |
Brand | TISCO ,BAOSTEEL,POSCO,JISCO,LISCO |
Certification | SGS,BV,IQI,TUV,ISO,etc |
Thickness | gauge 12(2.78 mm) |
Width | 1000 mm,1219 mm,1500 mm as per customers’ requirements |
Length | 2000, 3000, 6000 mm or as per customers’ requirements |
Surface | 2B; HL; Brush |
Standard | JIS,AISI,ASTM,GB,DIN |
Delivery time | About 15 -30 days or based on the sales contract |
MOQ | 1 Ton |
Advantages | has good corrosion resistance after exposure to temperatures in the chromium carbide precipitation range |
Product display :
Compaire Grade 304 and 321:
The intergranular corrosion tendency of 321 stainless steel is improved by adding TI to 304 stainless steel.
304 stainless steel plate and 321 stainless steel in the corrosion resistance of the difference is not big, but
in the heat condition of 500-600 degrees Celsius, most of the use of 321 stainless steel, because 321
stainless steel has TI as a stabilizing element, is also hot steel, make it has a better intergranular
corrosion resistance and high temperature strength, So it can be used to make the lining of wear-resistant
acid containers and wear-resistant equipment and conveying pipelines.
Chemical Composition:
Grade | C | Si | Mn | P | S | Ni | Cr | Mo |
321 | ≤0.08 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.03 | 9.00~13.00 | 17.00~19.00 | - |
Physical Property:
Grade | Tensile Strength(Mpa) | Yield Strength(Mpa) | Elongation(%) | HBW | HRB | HV |
321 | ≥520 | ≥205 | ≥40 | ≤187 | ≤90 | ≤200 |